ABSTRAK

The paper discussed the laboratory investigation of permanent deformation characteristics of asphalt concrete mixes containing reclaimed materials. The reclaimed materials used in this study were reclaimed plastic (HDPE) obtained from chopped plastic milk cartons and Reclaimed Asphalt Pavement (RAP). Reclaimed plastic was used to modify 60/70 penetration grade bitumen and Its effect on basic bitumen properties was tested over a range of test temperatures. The Marshall stability tests were carried out to determine the optimum bitumen content and optimum waste plastic content of asphalt concrete. The optimum waste plastic content in binder was found to be 1.5% by weight of binder. RAP contents of 30 and 60% were used to modify asphalt concrete mixes. The permanent deformation characteristics of asphalt concrete with and without reclaimed materials were evaluated in laboratory using Repeated Load Axial Test and Wheel Tracking Test at a range of test temperatures. The VESYS model was used to predict rutting characteristics for 10 years ahead. Test results showed that the asphalt concrete prepared using reclaimed materials such as waste plastic and Reclaimed Asphalt Pavement (RAP) were more resistance on permanent deformation over a range temperature.

Dibuat oleh : D. Woodward and A. Woodside, Imam Aschuri, MSc. (aschuri@itenas.ac.id)

Kata Kunci :

Keterangan :  Makalah ini  di muat pada  The Six International Conference on Maintenance and Rehabilitation of Pavement and Technological Control, Mairepav 6 Vol. 1, Politecnico Di Torino, Italy, July 8-10, 2009 ISBN : 978-88-8202-029-3

Permanent Deformation Characteristics of Asphalt Concrete Containing Reclaimed Materials